Hastelloy C276 suppliers in India

Alloy C276 Material, N10276 Nickel Alloy

Dealers & distributor of N10276 Material, 2.4819 material, 2.4819 steel, 2.4819 hastelloy, Din 2.4819. Check UNS N10276 chemical composition

Table of contents
Hastelloy c276 suppliers in India

N10276 Nickel Alloy Suppliers in Mumbai, India

Nirmaan Steel is only ISO 9001, 14001, 18001, PED and Govt. of India recognised Hastelloy c276 suppliers in India. Full testing & QC control Alloy C276/ N10276 Material & high quality assured. High Performance Corrosion resistance nickel alloy Hastelloy c276 material is available in many forms & shpae which includes:

Hastelloy C276 Pipe
Hastelloy C276 Tube
Hastelloy C276 Tubing
Hastelloy C276 Sheet
Hastelloy C276 Plate
Hastelloy C276 Round Bar
Hastelloy C276 Fasteners
Hastelloy C276 Bolts

Looking to buy Alloy 600 Tubing? Inconel 600 Tubing?

Check Today’s price of Alloy 600 Tubing in India

Alloy C276 Material Price Per Kg

Hastelloy C276 price per kg is Rs. 2800. In the UK therefore, the per kilo price of N10276 Material, would be roughly about 31.53 Pounds. But this does not indicate that Hastelloy Alloy C276 would be obtainable for the same price in other parts of the world like Japan, China, Singapore, USA, Europe, etc. Fact is, in China the price of N10276 Nickel Alloy could be 5% lesser than it is in India. On the other hand, It could cost around 35% more in the USA, than it costs in India. Of course, one thing has to be considered at all times, that the price is always changing.

Hastelloy C276 Price

Origin

Price in INR

(per kg)

Price in USD

(per kg)

Price in Euro

(per kg)

UNS N10276 Price in India

Indian

Rs 2800 – 2900/- as per your requirement sizes

$40

€34

Hastelloy 2.4819 material Price in Japan

Japanese

Rs 3600 – 3700/- as per your requirement sizes

$53

€45

2.4819 steel Price in UK / Europe

European

Rs 4100 – 4200/- as per your requirement sizes

$29

€25

2.4819 Hastelloy C276 Price in USA

USA

Rs 4600 – 4700/- as per your requirement size

$31

€26

Click here for complete (products, grade & size wise)

SPECIFICATIONS

UNS Number:

N10276

W.Nr.Number:

2.4819

Standards:

ASTM B564, B574, B575, B619, B622, B626, B366, B462, B775

Hastelloy C276 Welding Procedure

Hastelloy C276 welding procedure can be done by adopting different methods like GTA/TIG (Gas Tungsten Arc), MA/MIG (Gas Metal Arc) and SMA/Stick (Shielded Metal Arc). There are various other common welding techniques that are employed to weld Hastelloy C276 and these include RSW (resistance spot welding), EBW (electron beam welding), PAW (plasma arc welding) and LBW (laser beam welding). SAW (submerged arc welding) results in hot cracking and distortion, which is detrimental to Hastelloy C276 and that is why this welding technique is not used.

Hastelloy C276 Vs Alloy C4

With reference to Hastelloy C276 vs Alloy C4, Hastelloy C276 UNS is N10276. Alloy C4 has UNS N06455. The Chemical Composition of Hastelloy C276 is Silicon, Si 0.080, Iron, Fe 4-7, Cobalt, Co 2.50, Phosphorous, P 0.025, Manganese, Mn 1, Nickel, Ni 57, Carbon, C 0.010, Chromium, Cr 14.5-16.5, Tungsten, W 3-4.50, Molybdenum, Mo 15-17, Sulfur, S  0.010 and Vanadium, V 0.35. The Chemical Composition of Alloy C4 is Chromium: 16, Iron: 3 max., Titanium: 0.7 max., Carbon: 0.01 max., Manganese: 1 max., Cobalt: 2 max., Molybdenum: 16, Copper: 0.5 max., Silicon: 0.08 max., and Nickel: 65 balance. Alloy C4 has a Density of 0.312 lb/in3 (8.64 g/cm3). Hastelloy C276 has a Density of 0.321 lb/in³ (8.89 g/cm³).

Hastelloy c276 Density & Hardness

With reference to Hastelloy C276 Density & Hardness, the Density is 0.321 lb/in³ (8.89 g/cm³). The Rockwell B Hardness is 87. The Chemical Composition is Tungsten, W 3-4.50%, Nickel, Ni 57%, Phosphorous, P 0.025%, Chromium, Cr 14.5-16.5%, Iron, Fe 4-7%, Molybdenum, Mo 15-17%, Cobalt, Co 2.50%, Manganese, Mn 1%, Sulfur, S 0.010%, Silicon, Si 0.080%, Vanadium, V 0.35% and Carbon, C 0.010%. The Density is 8.89 g/cm³ (0.321 lb/in³). The Melting point is 2500 (1371 °C).

Hastelloy c276 Pressure Gauge & Temperature Rating

Hastelloy C276 Pressure Gauge & Temperature Rating can be measured by a manometer, which has a casing made of N10276 Nickel Alloy, to shield against corrosive chemicals. The Ultimate Tensile strength is 87200 psi (601.2 MPa). The Yield Strength is 29700 psi (204.8 MPa). Hastelloy C276 Elastic Modulus (RT) is 29700 ksi (205 GPa). The Elongation at Break is 56%. N10276 Material Rockwell B Hardness is 87. The Thermal Expansion co-efficient is 6.22 µin/in °F (11.2 µm/m °C). The Thermal Conductivity is 50.0 BTU in/hr.ft². °F (7.20 W/mK).

UNS N10276 chemical composition

Hastelloy C276 Chemical Composition

Hastelloy C276

Ni

C

Mo

Mn

Si

Fe

P

S

Co

Cr

Balance

0.010 max

15.00 – 17.00

1.00 max

0.08 max

4.00 – 7.00

0.04 max

0.03 max

2.5 max

14.50 – 16.50

Hastelloy C276 Mechanical Properties 
Typical Room Temperature Tensile Properties of Annealed Material

Product Form

Tensile (ksi)

.2% Yield (ksi)

Elongation %

Hastelloy C276 Bar

110.0

52.6

62

Hastelloy C276 Plate

107.4

50.3

67

Hastelloy C276 Sheet

115.5

54.6

60

Hastelloy C276 Tube & Alloy C276 Pipe

105.4

45.4

70

Hastelloy C276 Melting Point

Physical Properties

°F

British Units

°C

Metric Units

Density

72

0.321 lb./in.(3)

22

8.89 g/cm(3)

Melting Range

2415-

2500

 

1323-

1371

 

Electrical Resistivity

75

51 microhm-in.

24

1.30 microhm-m

Mean Coefficientof Thermal Expansion

75-200

6.2 microin./in

24-93

11.2 X 10(-6)m/m-K

75-400

6.7 microin./in

24-204

12.0 X 10(-6)m/m-K

75-600

7.1 microin./in

24-316

12.8 X 10(-6)m/m-K

75-800

7.3 microin./in

24-427

13.2 X 10(-6)m/m-K

75-1000

7.4 microin./in

24-538

13.4 X 10(-6)m/m-K

75-1200

7.8 microin./in

24-649

14.1 X 10(-6)m/m-K

75-1400

8.3 microin./in

24-760

14.9 X 10(-6)m/m-K

75-1600

8.8 microin./in

24-871

15.9 X 10(-6)m/m-K

75-1700

8.9 microin./in

24-927

16.0 X 10(-6)m/m-K

Thermal Conductivity

-270

50 Btu-in/ft²-hr

-168

7.2 W/m-K

-100

60 Btu-in/ft²-hr

-73

8.6 W/m-K

0

65 Btu-in/ft²-hr

32

9.4 W/m-K

100

71 Btu-in/ft²-hr

38

10.2 W/m-K

200

77 Btu-in/ft²-hr

93

11.1 W/m-K

400

90 Btu-in/ft²-hr

204

13.0 W/m-K

600

104 Btu-in/ft²-hr

316

15.0 W/m-K

800

117 Btu-in/ft²-hr

427

16.9 W/m-K

1000

132 Btu-in/ft²-hr

538

19.0 W/m-K

1200

145 Btu-in/ft²-hr

649

20.9 W/m-K

1400

159 Btu-in/ft²-hr

760

22.9 W/m-K

1600

173 Btu-in/ft²-hr

871

24.9 W/m-K

1800

185 Btu-in/ft²-hr

982

26.7 W/m-K

2000

195 Btu-in/ft²-hr

1093

28.1 W/m-K

Hastelloy C276 Equivalent

STANDARD

UNS

WERKSTOFF NR.

AFNOR

EN

JIS

BS

GOST

Hastelloy C276

N10276

2.4819

NiMo16Cr15W

NW 0276

ХН65МВУ

Special Steel

Scroll to Top