Hastelloy c22 suppliers
Alloy c22 material, UNS N06022 composition
Dealers & distributor of UNS N06022 wrought nickel alloy, 2.4602 material, Alloy N06022
Table of contents
C22 alloy material suppliers
Alloy c22 din 2.4602 Suppliers in Mumbai, India
Hastelloy C22 Pipe
Hastelloy C22 Tube
Hastelloy C22 Tubing
Hastelloy C22 Sheet
Hastelloy C22 Plate
Hastelloy C22 Bolts
Hastelloy C22 Fasteners
Looking to buy Alloy 600 Tubing? Inconel 600 Tubing?
Alloy C22 Price Per Kg
|
Hastelloy C22 Price |
Origin |
Price in INR (per kg) |
Price in USD (per kg) |
Price in Euro (per kg) |
|---|---|---|---|---|
|
UNS N06022 Price in India |
Indian |
Rs 2700 – 2800/- as per your requirement sizes |
$39 |
€33 |
|
Alloy c22 Price in Japan |
Japanese |
Rs 3500 – 3600/- as per your requirement sizes |
$52 |
€44 |
|
UNS N06022 wrought nickel alloy Price in UK / Europe |
European |
Rs 4000 – 4100/- as per your requirement sizes |
$59 |
€50 |
|
Alloy N06022 Price in USA |
USA |
Rs 4500 – 4600/- as per your requirement sizes |
$66 |
€57 |
Click here for complete (products, grade & size wise)
Hastelloy c22 Specifications
UNS Number:
N06022
W.Nr.Number:
2.4602
ASTM Standards:
B366, B462, B564, B574, B575, B619, B622, B626, B775
ASME Standards:
SB366, SB574, SB619, SB622, SB626, SFA5.14 (ERNiCRMo-10)
Hastelloy C22 Properties & Applications
Hastelloy C22 properties & applications are numerous. The applications of Alloy c22 material are cellophane manufacturing, chemical process industry, chlorination systems, waste water processing, flue gas scrubbers, chlorination systems, pesticide production, pharmaceutical industries, sulfur dioxide scrubbers, nuclear fuel reprocessing, pulp and paper bleach plants, incineration scrubber systems, pickling systems, etc. The Chemical Composition of UNS N06022 is Cobalt, Co 2.5% min, Chromium, Cr 20-22.5%, Phosphorus, P 0.02% max, Tungsten, W 2.5-3.5%, Molybdenum, Mo 12.5-14.5%, Iron, Fe 2-6%, Carbon, C 0.015% max, Vanadium, V 0.35% min, Manganese. Mn 0.5% max, Sulfur, S 0.02% max, Silicon, Si 0.08% max and Nickel, Ni remainder.
Alloy 22 Machinability
Alloy 22 machinability is easily achieved with the help of high-speed steel tooling. For turning or milling, carbide tools are employed. By the use of conventional coolants, it becomes possible to perform machining operations. The Density of Alloy 22 is 0.314 lb/in³ (8.69 g/cm³). The Melting Point of UNS N06022 Alloy is 2550 °F (1399 °C). Alloy c22 Thermal Conductivity (at 100 °C/212 °F) is 6.4 BTU in/hr.ft². °F (11.1 W/mK). The Elastic Modulus of UNS N06022 wrought nickel alloy is 29878 psi (206 MPa). 2.4602 material Mean Coefficient of Thermal Expansion at 24 to 93 °C (75 to 200 °F) is 12.4 μm/m. °C (6.9 μm/in.- °F).
Hastelloy C22 Annealing
Hastelloy C22 annealing can be achieved at temperatures ranging between 2020-2150 °F and this should be followed up with a rapid quench. The Specific Heat Capacity of Alloy N06022 is 414 J/Kg-K (0.099 Btu/lb.-°F). The Magnetic Permeability of alloy c22 din 2.4602 at 200 oersted (15.9 kA/m) is ≤1.001. The Electrical Resistivity of C22 alloy material is 1.215 µΩm (730.7 µΩm•circ mil/ft). c22 alloy steel has several outstanding characteristics such as it shows tremendous resistance to stress corrosion cracking, crevice corrosion, pitting, oxidizing and reducing media, chemical process environments, oxidizing aqueous media, acids, seawater, etc. Alloy c22 material also has exceptional weldability features.
UNS N06022 composition
Hastelloy C22 Chemical Composition
Hastelloy C22 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr |
Balance | 0.010 max | 12.5 – 14.5 | 0.50 max | 0.08 max | 2 – 6 | 0.02 max | 0.02 max | 2.5 max | 20 – 22.5 |
Hastelloy C22 Mechanical Properties
Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
8.69 g/cm3 | 1399 °C (2550 °F) | Psi – 45000 , MPa – 310 | Psi – 1,00,000 , MPa – 690 | 45 % |
1399 °C (2550 °F)
In what forms is Hastelloy C22 Available at Nirmaan Steel?
- Sheet
- Plate
- Bar
- Pipe & Tube (welded & seamless)
- Fittings (i.e. flanges, slip-ons, blinds, weld-necks, lapjoints, long welding necks, socket welds, elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples)
- Wire
Hastelloy C22 Chemical Composition, %
C | Cr | Co | Fe | Mn | Mo | Ni | P |
|---|---|---|---|---|---|---|---|
.010 max | 20-22.5 | 2.5 max | 2.0-6.0 | .50 max | 12.5-14.5 | Balance | .02 max |
Si | S | W | V | ||||
.08 max | .02 max | 2.5-3.5 | .35 max |
ASTM Specifications of Hastelloy C22 Products
Pipe Smls | Pipe Welded | Tube Smls | Tube Welded | Sheet/Plate | Bar | Forging | Fitting |
|---|---|---|---|---|---|---|---|
B622 | B619 | B622 | B626 | B575 | B574 | B564 | B366 |
STANDARD | UNS | WERKSTOFF NR. | AFNOR | EN | JIS | BS | GOST |
Hastelloy C22 | N06022 | 2.4602 | – | NiCr21Mo14W | NW 6022 | – | – |
Special Steel
- Carbon Steel Pipe
- ASTM A106 Grade B Pipe
- ASTM A53 Grade B Pipe
- ASTM A333 Grade 6 Pipe
- IS 4923 Steel Pipes
- ASTM A179 Pipe
- ASTM A192 Tube
- BS 3059 Boiler Tube
- SA 210 Boiler Tube
- DIN 2391 ST 52
- ASTM A671 Pipe
- ASTM A671 Grade CC60
- ASTM A671 Grade CC65
- ASTM A671 Grade CC70
- ASTM A672 Pipe
- ASTM A672 Grade C55
- ASTM A672 Grade C60
- ASTM A672 Grade C65
- ASTM A672 Grade C70